Many of the salt spray corrosion test methods developed over the last 10-15 years have included controlled relative humidity and precisely-defined transitions between wet and dry conditions. In this webinar, we will discuss why this has occurred and show some examples of test results that were significantly impacted by differences in wetting and drying rates. We will talk about the concept of deliquescence, why it is important, and how it is controlled in some of these newer test methods.